Table 2 Wetting and surface energy characterization

From: Printed paper-based arrays as substrates for biofilm formation

Surface

θ r [°]

Surface energy [mN/m]

Water

DIM

EG

γ s p

γ s d

γ s

Latex 1

84 ± 1

52 ± 1

73 ± 1

3.4

27.8

31.2

Latex 2

74 ± 3

47 ± 2

59 ± 2

6.6

31.3

37.9

Kaolin

64 ± 2

50 ± 1

48 ± 1

12.2

29.9

42.1

PCC

92 ± 3

52 ± 1

52 ± 2

1.4

34.7

36.1

PS (96-well)

80 ± 1b

37 ± 2b

53 ± 2b

3.2

38.2

41.4

PDMSa

114 ± 1b

92 ± 2b

96 ± 1b

0.6

11.7

12.3

  1. aNot corrected for roughness, b(Juvonen et al. [2013]).