Molecular weight before and after enzyamatic hydrolysis. Reactions (1 ml) were performed at 70 °C for 3 days using Cut190*SS, one piece of 6 mm PET-GF film and 100 mM HEPES buffer (pH 8.5), as described in “Materials and methods”. Degradation rates of reactions 1 and 2 were 33.6 and 31.4%, respectively. Mn: number-average molecular weight. Mw: weight-average molecular weight