Fig. 1

a SEM-image of a glass substrate coated with copper filled TiO2 (Cu-TiO2). b Distribution of the TiKα1 signal of the copper-filled TiO2-coating resulting from SEM/EDX investigation. c Distribution of the CuKα signal of the copper-filled TiO2-coating